Breviary Technical Ceramics

 

      Joining and Bonding Techniques

 

 


   

8.2.3.3 Further Applications

  • High-voltage insulator
    Fixing the mounting of an insulator subject to tensile or compressive stress.

  •  

Figure 207: Cemented joint

  • Coupling ring wheel
    Reinforcing a plastic

    o epoxy resin, ceramic filled
    o hardening conditions: 180 °C, 30 min
    o working temperature 220 °C

 


Figure 208: Coupling ring wheel

  • Slotted thread guide
    Precisely reinforcing the wear location on a component

    o 2-component glue
    o hardening conditions: 80 °C, 1 h
    o working temperature 100 °C


Figure 209: Slotted thread guide

 

 
 
<< back   home   next >>